What a piping inspection covers

  • External visual inspection of piping, supports, hangers, guides, coatings and insulation
  • Corrosion under insulation (CUI) screening and follow-up where the temperature range and condition call for it
  • Injection points and mix points, inspected as their own circuits
  • Deadlegs, where stagnant product concentrates corrosion
  • Soil-to-air interfaces and buried piping transitions
  • Small-bore connections and threaded fittings prone to vibration fatigue
  • Ultrasonic thickness at CMLs, and profile radiography where insulation stays on

Circuits make the data mean something

A piping system is divided into circuits of similar material, service and expected damage. Each circuit gets its own isometric drawing, its own CMLs and its own corrosion rate. Without good circuits, a fast-corroding section hides inside a slow average and the inspection date is wrong.

How often piping is inspected

API 570 sets maximum intervals by piping class. Class 1 piping, with the highest consequence of a leak, gets thickness measurements at least every five years. Class 2 and Class 3 piping is measured at least every ten years. Thickness intervals are also limited to half the remaining life. External visual inspections follow their own schedule by class, and risk-based inspection can set intervals differently.

Why my background matters here

I've worked as a pipefitter and welded piping for years before inspecting it. I know how piping actually gets built and repaired in the field, which is where most of the surprises come from.

Working across the Appalachian region: Kentucky, West Virginia, Virginia, Tennessee, North Carolina, South Carolina and southern Pennsylvania.