What a pressure vessel inspection covers
- External visual inspection of the shell, heads, nozzles, supports, anchor bolts, ladders and platforms, insulation and coatings
- Internal visual inspection of the shell, heads, internals, welds, linings and any previous repairs
- On-stream inspection when the vessel can't be taken out of service, with the damage mechanisms and data to justify it
- Ultrasonic thickness readings at condition monitoring locations (CMLs) on the shell, heads and nozzles
- Weld and nozzle inspection, with MT, PT, shear-wave UT or radiography where the damage mechanism calls for it
- Pressure-relief device records and service history
How often a pressure vessel is inspected
Under API 510, the internal or on-stream inspection interval is the lesser of ten years or half the vessel's remaining life, unless a risk-based inspection program sets it. The external inspection is due at the lesser of five years or the internal interval. Jurisdictions and owner programs can be stricter, so the governing rule is whichever is tightest.
The interval is only as good as the thickness data and corrosion rates behind it. A wrong reading or a CML in the wrong place moves the due date, sometimes in the wrong direction.
What the inspection should produce
- Measured thickness against required thickness at every CML
- Short-term and long-term corrosion rates, remaining life and MAWP
- The next inspection dates, with the reason for each
- Clear findings and recommendations, each with a priority and due date
- Repair and alteration requirements under API 510 and the National Board Inspection Code
Why my background matters here
Before I ever inspected a pressure vessel, I spent years as a boilermaker welding them. I know where repairs have typically been made, where fit-up gets forced and where a weld is most likely to be hiding something. That's where I look first.
Working across the Appalachian region: Kentucky, West Virginia, Virginia, Tennessee, North Carolina, South Carolina and southern Pennsylvania.